Ceramic Blades & Sharpeners

Long-Life and Precision with Ceramic Blades and Sharpeners

Fine-grained ceramics are ideal for cutting tools. Using ceramic materials substantially increase blade life and precision due to their inherent strength and wear resistance. Precision machining is available to deliver complete parts – or we can supply blanks for your machining.

Applications:

  • Capsule cutters (Pharmaceutical)
  • Medical device blades
  • Exacto-style blades and cutters
  • Large ceramic trimmer blades
  • Receipt cutters for registers and point-of-sale use
  • Knife sharpeners

 

Image of ceramic blades

benefits

Ceramic blades have excellent wear and corrosion resistance allowing them to hold their edge for dramatically a increased lifetime. For example our Norzide® zirconia lasts 20% longer than tungsten carbide. Other benefits include:

  • Up to 100x lifetime compared to standard steel
  • Electrically resistant with ESD options
  • Corrosion resistant
  • High strength

blades

Our blades can be constructed from any of our material compositions. The CeraShear™ family is engineered specially for blades. Their benefits include:

  • Greater mechanical strength than tungsten carbide
  • Absence of metal phase for improving corrosion wear
  • Fine-grain structures allows for finishes <1μm

sharpeners

In addition to ceramic blades, CoorsTek offers ceramic sharpening blocks. Each ceramic is extremely hard, and can be used to sharpen any blade, allowing for precise honing and and excellent finishes.