Alumina 85

Composition

Nom 85% Al2O3 

Description

Reliable, economic, general use technical ceramic.
This alumina exhibits good wear and corrosion resistance in addition to being electrically insulative.

Example Applications

  • Mill linings
  • Electrostatic precipitator insulators

CoorsTek Formulations

Contact a CoorsTek expert to choose an Alumina 85 solution for your application.

Columns
Property Units Value

Flexural Strength MOR, (20°C)

MPa

290-310

Compressive Strength, (20°C)

MPa

1550-2000

Fracture Toughness, KIc

MPa m1/2

3.0-4.0

Hardness, Rockwell 45N

R45N

73-76

Hardness, Knoop 1000gm

GPa

9.4

Maximum Use Temperature

°C

1250-1400

Coefficient of Thermal Expansion, (25-1000°C)

1 x 10-6/°C

7.2

Thermal Shock Resistance, (∆T)

°C

300

Thermal Conductivity, (20°C)

W/m K

13.8-16.7

Dielectric Strength, (6.35mm)

ac-kV/mm

9.4-10.0

Dielectric Constant, (1 MHz)

25°C

8.2-8.5

Volume Resistivity, (25°C)

ohm-cm

>1014

The information provided on this chart is for general material property reference only.  The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.