Alumina 90

Composition

Nom 90% Al2O3

Description

Excellent ceramic for abrasive environments where superior wear properties are required.

Example Applications

  • Grinding media
  • Rod & ball media
     

CoorsTek Formulations

Contact a CoorsTek expert to choose an Alumina 90 solution for your application.

Columns
Property Units Value

Flexural Strength MOR, (20°C)

MPa

250-365

Compressive Strength, (20°C)

MPa

2400-2482

Fracture Toughness, KIc

MPa m1/2

3.0-4.0

Hardness, Rockwell 45N

R45N

75-78

Hardness, Knoop 1000gm

GPa

10.4-10.8

Maximum Use Temperature

°C

920-1045

Coefficient of Thermal Expansion, (25-1000°C)

1 x 10-6/°C

7.5-8.5

Thermal Shock Resistance, (∆T)

°C

250

Thermal Conductivity, (20°C)

W/m K

12.6-24.0

Dielectric Strength, (6.35mm)

ac-kV/mm

5.3-8.3

Dielectric Constant, (1 MHz)

25°C

8.8-22.0

Volume Resistivity, (25°C)

ohm-cm

> 1014

The information provided on this chart is for general material property reference only.  The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.