Zirconia Toughened Alumina

Composition

10% ZTA Min

Description

Specialized alumina designed for high thermal shock resistance and increased toughness.

Example Applications

  • Bushings
  • Wire bonding capillaries
     

CoorsTek Formulations

Contact a CoorsTek expert to choose a Zirconia Toughened Alumina solution for your application.

  • 12+ unique compositions manufactured globally
Columns
Property Units Value

Flexural Strength MOR, (20°C)

MPa

450-1250

Compressive Strength, (20°C)

MPa

1975-2900 

Fracture Toughness, KIc

MPa m1/2

3 .0-76.0

Hardness, Rockwell 45N

R45N

75-85

Hardness, Knoop 1000gm

GPa

11.5-16.1

Maximum Use Temperature

°C

1400-1500

Coefficient of Thermal Expansion, (25-1000°C)

1 x 10-6/°C

8.0-9.0

Thermal Shock Resistance, (∆T)

°C

225-500

Thermal Conductivity, (20°C)

W/m K

17.0-27.0

Dielectric Strength, (6.35mm)

ac-kV/mm

9.0 

Dielectric Constant, (1 MHz)

25°C

9.8-10.6

Volume Resistivity, (25°C)

ohm-cm

1013-> 1014

The information provided on this chart is for general material property reference only.  The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.