Composition

99.9% Al2O3

dESCRIPTION

As a result of its high purity, crystal structure, and uniform grain size, Sapphal™ Alumina is extremely inert and visibly translucent. CoorsTek has the capability to manufacture custom Sapphal alumina components in large and complex geometries. 

Download the Semiconductor Oxides Material Properties Chart

Download the Semiconductor Advanced Alumina Brochure

Columns
Property Units Value

Minor Chemistry, (Total)

ppm weight

500

Grain Size

μm

2-50

Flexural Strength (MOR), 3-point

MPa

350

Flexural Strength (MOR), 4-point

MPa

285

Fracture Toughness, KIc

MPa-m1/2

4-5

Hardness, Vickers 500g

GPa

18

Hardness, Vickers 1000g

GPa

17

Elastic Modulus

GPA

390

Coefficient of Thermal Expansion, (25°C-1000°C)

1 x 10-6/°C

8.3

Thermal Conductivity

W/m-K

35

Dielectric Strength, (1 mm)

ac-kV/mm

18.5

Volume Resistivity, (25°C)

ohm-cm

>1015

Volume Resistivity, (500°C)

ohm-cm

8x1011

Volume Resistivity, (1000°C)

ohm-cm

1010

Dielectric Constant, (1 MHz)

10

Dielectric Loss (tan δ), (1 MHz)

10-3

The information provided on this chart is for general material property reference only.  The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.