Home

+1 303 271 7100

Contact

Synthetic Quartz

Composition

SiO2

Description

CoorsTek synthetic fused quartz delivers exceptional thermal shock resistance and high purity — making it an an excellent material for crucibles used in single silicon crystal pulling and other semiconductor applications. 

Columns
Property Units Value

Minor Chemistry, (Total)

ppm weight

30

Flexural Strength (MOR), 3-point

 

MPa

128

Flexural Strength (MOR), 4-point

MPa

104

Fracture Toughness, KIc

MPa-m1/2

1.1

Hardness, Vickers 500g

GPa

6

Hardness, Vickers 1000g

GPa

5

Coefficient of Thermal Expansion, (25°C-1000°C)

1 x 10-6/°C

0.4

Dielectric Strength, (1 mm)

ac-kV/mm

31.4

Volume Resistivity, (25°C)

ohm-cm

>1014

Volume Resistivity, (25°C)

ohm-cm

3x1011

Volume Resistivity, (25°C)

ohm-cm

9x109

Dielectric Constant, (1 MHz)

3.8

Dielectric Loss (tan δ), (1 MHz)

<10-4

The information provided on this chart is for general material property reference only.  The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.